The Resource Chloride-assisted stress-corrosion cracking in type 316 stainless steel water and gas-sampling tubes from the HYGAS pilot plant : failure analysis report, by Steven Danyluk and Gabriel M. Dragel, Materials Science Division

Chloride-assisted stress-corrosion cracking in type 316 stainless steel water and gas-sampling tubes from the HYGAS pilot plant : failure analysis report, by Steven Danyluk and Gabriel M. Dragel, Materials Science Division

Label
Chloride-assisted stress-corrosion cracking in type 316 stainless steel water and gas-sampling tubes from the HYGAS pilot plant : failure analysis report
Title
Chloride-assisted stress-corrosion cracking in type 316 stainless steel water and gas-sampling tubes from the HYGAS pilot plant
Title remainder
failure analysis report
Statement of responsibility
by Steven Danyluk and Gabriel M. Dragel, Materials Science Division
Creator
Contributor
Author
Subject
Language
eng
Cataloging source
GPO
http://library.link/vocab/creatorName
Danyluk, Steven
Government publication
federal national government publication
Illustrations
illustrations
Index
no index present
Literary form
non fiction
Nature of contents
bibliography
http://library.link/vocab/relatedWorkOrContributorName
  • Dragel, Gabriel M.
  • Argonne National Laboratory
Series statement
ANL/MSD/FE ; 77-9
http://library.link/vocab/subjectName
  • Stainless steel
  • Tubes
  • Chlorides
Label
Chloride-assisted stress-corrosion cracking in type 316 stainless steel water and gas-sampling tubes from the HYGAS pilot plant : failure analysis report, by Steven Danyluk and Gabriel M. Dragel, Materials Science Division
Instantiates
Publication
Note
  • Prepared for the U.S. Dept. of Energy under contract no. W-31-109-Eng-38
  • Dec. 1977
Bibliography note
Includes bibliographical references
Carrier category
volume
Carrier category code
nc
Carrier MARC source
rdacarrier
Content category
text
Content type code
txt
Content type MARC source
rdacontent
Control code
17004242
Dimensions
28 cm.
Extent
16 pages
Media category
unmediated
Media MARC source
rdamedia
Media type code
n
Other physical details
illustrations
Label
Chloride-assisted stress-corrosion cracking in type 316 stainless steel water and gas-sampling tubes from the HYGAS pilot plant : failure analysis report, by Steven Danyluk and Gabriel M. Dragel, Materials Science Division
Publication
Note
  • Prepared for the U.S. Dept. of Energy under contract no. W-31-109-Eng-38
  • Dec. 1977
Bibliography note
Includes bibliographical references
Carrier category
volume
Carrier category code
nc
Carrier MARC source
rdacarrier
Content category
text
Content type code
txt
Content type MARC source
rdacontent
Control code
17004242
Dimensions
28 cm.
Extent
16 pages
Media category
unmediated
Media MARC source
rdamedia
Media type code
n
Other physical details
illustrations

Library Locations

    • Indiana State LibraryBorrow it
      315 W. Ohio St., Indianapolis, IN, 46202, US
      39.77004 -86.164015

Library Links

Processing Feedback ...